The production method of silicon aluminum barium calcium is to mix silica, bauxite and coke evenly, add them into the submerged arc furnace for smelting, and produce silicon aluminum alloy. Then CaO and coke are added in batches to promote the formation of silicon, calcium and aluminum. Then barium ore and coke are added in batches to promote the formation of silicon calcium barium aluminum alloy. Generally, the composition of silicon calcium barium aluminum alloy is: Si>30%, Ca>6%, Ba>9%, Al>8%.
During production, the ratio of Al2O3/SiO2, CaO/BaO, (CaO+BaO)/SiO2 should be controlled, and the amount of coke added should be controlled.
The equipment parameters shall be higher current and lower working voltage, with higher polar circle power and higher furnace power. Keep the reaction zone in the furnace at a high temperature. The method of braising and burning shall be adopted from beginning to end, and CaO and BaO shall be added to treat the slags, so as to eliminate them from the furnace.
For example, when producing silicon calcium barium in large electric furnace, the method of hot punching aluminum ingot can be used to produce silicon calcium barium aluminum alloy. However, this method is not as economical as using ore to produce silicon calcium barium aluminum alloy.